峰值应力对Ti6242压气机盘锻件室温保载效应的影响 |
徐小严, 方超, 邱建科, 张蒙蒙, 史栋刚, 马英杰, 雷家峰, 杨锐 |
Influence of Peak Stress on Room Temperature Dwell Effect in Ti6242 Compressor Disc Forging |
XU Xiaoyan, FANG Chao, QIU Jianke, ZHANG Mengmeng, SHI Donggang, MA Yingjie, LEI Jiafeng, YANG Rui |
图5 不同峰值应力下Ti6242合金常规疲劳和保载疲劳断口上准解理小平面的空间取向分布 |
Fig.5 Distributions of spatial orientations of the quasi-cleavage facets on NF (a) and DF (b) fractures of Ti6242 alloy at various peak stresses (θ—angle between the facet normal and stress axis) |
![]() |