6061铝合金搅拌摩擦增材制造显微组织演变及力学性能 |
||||||||||||||||||||||
| 杨帆, 裴世超, 罗新蕊, 陈宇翔, 李宁宇, 常永勤 | ||||||||||||||||||||||
|
Microstructure Evolution and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Friction Stir Additive Manufacturing |
||||||||||||||||||||||
| YANG Fan, PEI Shichao, LUO Xinrui, CHEN Yuxiang, LI Ningyu, CHANG Yongqin | ||||||||||||||||||||||
| 表1 6061铝合金母材及FSAM试样不同位置的平均晶粒尺寸和晶界含量 |
||||||||||||||||||||||
| Table 1 Average grain sizes and number fractions of LAGBs and HAGBs in 6061 aluminum alloy BM and the different locations shown in Fig.3a |
||||||||||||||||||||||
|
||||||||||||||||||||||