6061铝合金搅拌摩擦增材制造显微组织演变及力学性能 |
| 杨帆, 裴世超, 罗新蕊, 陈宇翔, 李宁宇, 常永勤 |
|
Microstructure Evolution and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Friction Stir Additive Manufacturing |
| YANG Fan, PEI Shichao, LUO Xinrui, CHEN Yuxiang, LI Ningyu, CHANG Yongqin |
| 图15 PWHT态试样中不同析出相的TEM明场像及对应的选区电子衍射花样 |
| Fig.15 TEM bright field images and corresponding selected area electron diffraction (SAED) patterns (insets) of rod-like (a) and spherical (b) precipitates for 6061 aluminum alloy fabricated by FSAM followed by PWHT |
|