6061铝合金搅拌摩擦增材制造显微组织演变及力学性能 |
杨帆, 裴世超, 罗新蕊, 陈宇翔, 李宁宇, 常永勤 |
Microstructure Evolution and Mechanical Properties of 6061 Aluminum Alloy Fabricated by Friction Stir Additive Manufacturing |
YANG Fan, PEI Shichao, LUO Xinrui, CHEN Yuxiang, LI Ningyu, CHANG Yongqin |
图6 6061铝合金母材及FSAM试样在Euler角φ2 = 0°和φ2 = 45°的取向分布函数(ODF)图及织构分布 |
Fig.6 Orientation distribution function (ODF) maps and texture distributions (Black dots in Figs.6a1-a4 and b1-b4 corres-pond to the positions of the textures in Figs.6c and d, respectively) (a1-a4) ODF maps for BM (a1), FSAM-1 (a2), FSAM-2 (a3), and FSAM-3 (a4) at Euler angle φ2 = 0° (b1-b4) ODF maps for BM (b1), FSAM-1 (b2), FSAM-2 (b3), and FSAM-3 (b4) at φ2 = 45° (c) texture at φ2 = 0° (Φ, φ1—Euler angles) (d) texture at φ2 = 45° |
![]() |