表3 焊缝金属(WM)的实测化学成分(MA) (mass fraction / %)
Table 3 Chemical compositions of weld metals (WMs) (MA)
WM numberCSiMnNiAlTiMoOFe
WM10.1020.2062.0800.6600.0370.0410.0640.022Bal.
WM20.0900.2052.0300.6340.0330.0440.0700.024Bal.
WM30.0890.2011.8600.6570.0260.0480.0510.025Bal.
WM40.0870.1851.8200.6120.0210.0590.0640.027Bal.
WM50.0860.1651.7900.6030.0210.0630.0590.029Bal.