CaF2-TiO2 焊剂作用下EH36船板钢气电立焊焊缝金属组织优化及力学性能调控 |
| 谢旭, 万一博, 钟明, 邹晓东, 王聪 |
|
Optimizing Microstructures and Mechanical Properties of Electro-Gas Welded Metals for EH36 Shipbuilding Steel Treated by CaF2-TiO2 Fluxes |
| XIE Xu, WAN Yibo, ZHONG Ming, ZOU Xiaodong, WANG Cong |
| 图3 不同WM中夹杂物内Ti、Si和Mn元素的归一化原子百分比 |
| Fig.3 Normalized atomic fractions of Ti, Si, and Mn of inclusions in different WMs (a) WM1 (b) WM2 (c) WM3 (d) WM4 (e) WM5 |
|