CaF2-TiO2 焊剂作用下EH36船板钢气电立焊焊缝金属组织优化及力学性能调控 |
| 谢旭, 万一博, 钟明, 邹晓东, 王聪 |
|
Optimizing Microstructures and Mechanical Properties of Electro-Gas Welded Metals for EH36 Shipbuilding Steel Treated by CaF2-TiO2 Fluxes |
| XIE Xu, WAN Yibo, ZHONG Ming, ZOU Xiaodong, WANG Cong |
| 图2 WM中典型夹杂物形貌的SEM像以及相应的EDS元素分析结果 |
| Fig.2 SEM images and corresponding EDS results (atomic fraction, %) of typical inclusions in WMs (a) O-Ti-Al-Mn-Si (b) O-Ti-Al-Mn-Si-S (c) O-Ti-Al-Mn |
|