偏滤器用钨基材料的热负荷损伤行为研究进展 |
| 罗来马, 陈宇, 姚刚, 朱晓勇, 朱大焕, 吴玉程 |
|
Research Progress on Heat Load Damage Behavior of Tungsten-Based Materials for Divertor |
| LUO Laima, CHEN Yu, YAO Gang, ZHU Xiaoyong, ZHU Dahuan, WU Yucheng |
| 图10 不同功率密度下W-2.0%Y2O3复合材料经100次脉冲热负荷实验后的横向-法向(TD-ND)和轧向-横向(RD-TD)表面形貌[ |
| Fig.10 Low (a-d) and high (a1-d1) magnified SEM images showing surface morphologies of the W-2.0%Y2O3 composite material after 100 pulses thermal shock experiment with different power densities[ (a, a1, b, b1) TD-ND surfaces (c, c1, d, d1) RD-TD surfaces |
|