偏滤器用钨基材料的热负荷损伤行为研究进展 |
| 罗来马, 陈宇, 姚刚, 朱晓勇, 朱大焕, 吴玉程 |
|
Research Progress on Heat Load Damage Behavior of Tungsten-Based Materials for Divertor |
| LUO Laima, CHEN Yu, YAO Gang, ZHU Xiaoyong, ZHU Dahuan, WU Yucheng |
| 图7 不同高功率密度加载下W-V合金的SEM像[ |
| Fig.7 Low and high (insets) magnified SEM images of the loaded surfaces under different high heat flux (HHF) densities[ (a-c) W-1V alloy (d-f) W-5V alloy (g-i) W-10V alloy |
|