偏滤器用钨基材料的热负荷损伤行为研究进展 |
| 罗来马, 陈宇, 姚刚, 朱晓勇, 朱大焕, 吴玉程 |
|
Research Progress on Heat Load Damage Behavior of Tungsten-Based Materials for Divertor |
| LUO Laima, CHEN Yu, YAO Gang, ZHU Xiaoyong, ZHU Dahuan, WU Yucheng |
| 图3 主裂纹和二次裂纹典型分布以及不同加载条件下纯W表面开裂情况的SEM像[ |
| Fig.3 SEM images showing typical distribution of primary and secondary cracks (a) and cracking on the pure W surface under different heat loads with 1 pulse (b-d)[ (b) 0.5 GW/m2 (c) 0.85 GW/m2 (d) 1.25 GW/m2 |
|