偏滤器用钨基材料的热负荷损伤行为研究进展 |
罗来马, 陈宇, 姚刚, 朱晓勇, 朱大焕, 吴玉程 |
Research Progress on Heat Load Damage Behavior of Tungsten-Based Materials for Divertor |
LUO Laima, CHEN Yu, YAO Gang, ZHU Xiaoyong, ZHU Dahuan, WU Yucheng |
图2 加载3 GW/m2热负荷后W样品表面的SEM像[ |
Fig.2 Surface SEM images of cracked and melted zones in W after 3 GW/m2 heat loads[ (a) 104 pulse of 1 ms at 20 Hz (b1, b2) high magnified SEM images of Fig.2a (c, d) 1 pulse of 13 ms (c) and 14 ms (d), respectively |
![]() |