Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响 |
||||||||||||
| 何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰 | ||||||||||||
|
Effect of Al2O3 Coating on Interface Reaction Between Si-Based Ceramic Core and Ni-Based Single-Crystal Superalloy |
||||||||||||
| HE Jiabao, WANG Liang, ZHANG Chaowei, ZOU Mingke, MENG Jie, WANG Xinguang, JIANG Sumeng, ZHOU Yizhou, SUN Xiaofeng | ||||||||||||
| 表4 合金/不同硅基陶瓷体系的润湿角 |
||||||||||||
| Table 4 Wetting angles of superalloy/different Si-based ceramic core systems |
||||||||||||
|
||||||||||||