Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响
何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰

Effect of Al2O3 Coating on Interface Reaction Between Si-Based Ceramic Core and Ni-Based Single-Crystal Superalloy
HE Jiabao, WANG Liang, ZHANG Chaowei, ZOU Mingke, MENG Jie, WANG Xinguang, JIANG Sumeng, ZHOU Yizhou, SUN Xiaofeng
表2 图7b中点1和2的EDS结果 (mass fraction / %)
Table 2 EDS results of points 1 and 2 in Fig.7b
PointAlONiSiCoCrReMoWTaHfC
10.620.5820.052.247.770.6223.243.7124.766.853.845.73
20.140.519.100.602.830.4039.4134.584.063.584.81