Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响 |
何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰 |
Effect of Al2O3 Coating on Interface Reaction Between Si-Based Ceramic Core and Ni-Based Single-Crystal Superalloy |
HE Jiabao, WANG Liang, ZHANG Chaowei, ZOU Mingke, MENG Jie, WANG Xinguang, JIANG Sumeng, ZHOU Yizhou, SUN Xiaofeng |
图16 界面反应后镍基单晶高温合金底部和未表面改性的硅基陶瓷型芯表面的XRD谱 |
Fig.16 XRD spectra of the Ni-based single-crystal superalloy bottom (a) and the unmodified Si-based ceramic core surface (b) after interface reaction |
![]() |