Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响
何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰

Effect of Al2O3 Coating on Interface Reaction Between Si-Based Ceramic Core and Ni-Based Single-Crystal Superalloy
HE Jiabao, WANG Liang, ZHANG Chaowei, ZOU Mingke, MENG Jie, WANG Xinguang, JIANG Sumeng, ZHOU Yizhou, SUN Xiaofeng
图15 未表面改性的硅基陶瓷型芯与镍基单晶高温合金反应后硅基陶瓷型芯表面形貌SEM像及EDS元素面分布
Fig.15 Low (a) and high (b) magnified SEM images showing surface morphologies of the unmodified Si-based ceramic core after reaction with the Ni-based single-crystal superalloy and EDS mappings corresponding to Fig.15a (c, d)