Al2O3 涂层对硅基陶瓷型芯与镍基单晶高温合金界面反应的影响
何家宝, 王亮, 张朝威, 邹明科, 孟杰, 王新广, 姜肃猛, 周亦胄, 孙晓峰

Effect of Al2O3 Coating on Interface Reaction Between Si-Based Ceramic Core and Ni-Based Single-Crystal Superalloy
HE Jiabao, WANG Liang, ZHANG Chaowei, ZOU Mingke, MENG Jie, WANG Xinguang, JIANG Sumeng, ZHOU Yizhou, SUN Xiaofeng
图2 施加Al2O3涂层的硅基陶瓷型芯的形貌及EDS元素面分布
Fig.2 Surface morphologies (a, b) and EDS elemental analyses of Al2O3-coated Si-based ceramic core
(a) overall morphology
(b) microstructure of the Al2O3-coated Si-based ceramic core (c-f) EDS mappings corresponding to Fig.2b