锆合金氧化膜中相变与裂纹演化的相场模拟
|
|
王小齐, 张金虎, 郭辉, 李学雄, 许海生, 柏春光, 徐东生, 杨锐
|
Phase-Field Simulations of Phase Transformation and Crack Evolution in Zirconium Alloy Oxide Film
|
|
WANG Xiaoqi, ZHANG Jinhu, GUO Hui, LI Xuexiong, XU Haisheng, BAI Chunguang, XU Dongsheng, YANG Rui
|
|
表2 弹性能计算所需相关参数[24]
|
Table 2 Parameters employed in elastic energy calculation[24]
|
|
| Parameters | Symbol | Value |
|---|
| Young's modulus of t-ZrO2 | | 212 GPa | | Young's modulus of m-ZrO2 | | 241 GPa | | Poisson's ratio of t-ZrO2 | | 0.33 | | Poisson's ratio of m-ZrO2 | | 0.29 | | Eigenstrain of t-ZrO2 | (t-ZrO2) | | | Eigenstrain of m-ZrO2 | (m-ZrO2) | | Eigenstrain of t-ZrO2 (after 90° rotation about Y axis) | (t-ZrO2) | | Eigenstrain of m-ZrO2 (after 90° rotation about Y axis) | (m-ZrO2) | |
|
|
|