锆合金氧化膜中相变与裂纹演化的相场模拟 |
王小齐, 张金虎, 郭辉, 李学雄, 许海生, 柏春光, 徐东生, 杨锐 |
Phase-Field Simulations of Phase Transformation and Crack Evolution in Zirconium Alloy Oxide Film |
WANG Xiaoqi, ZHANG Jinhu, GUO Hui, LI Xuexiong, XU Haisheng, BAI Chunguang, XU Dongsheng, YANG Rui |
图10 相场模拟垂直氧化物-金属界面的裂纹演化 |
Fig.10 Phase-field simulation of crack perpendicular to the oxide-metal interface (ϕ—phase-field order parameter) (a) initial crack (b) crack reaches interface (c) crack propagates parallel to interface (d) force-displacement curve |
![]() |