锆合金氧化膜中相变与裂纹演化的相场模拟 |
王小齐, 张金虎, 郭辉, 李学雄, 许海生, 柏春光, 徐东生, 杨锐 |
Phase-Field Simulations of Phase Transformation and Crack Evolution in Zirconium Alloy Oxide Film |
WANG Xiaoqi, ZHANG Jinhu, GUO Hui, LI Xuexiong, XU Haisheng, BAI Chunguang, XU Dongsheng, YANG Rui |
图9 垂直于氧化物-金属界面的裂纹模型示意图 |
Fig.9 Schematic of crack perpendicular to the oxide-metal interface (unit: mm) |
![]() |