锆合金氧化膜中相变与裂纹演化的相场模拟 |
| 王小齐, 张金虎, 郭辉, 李学雄, 许海生, 柏春光, 徐东生, 杨锐 |
|
Phase-Field Simulations of Phase Transformation and Crack Evolution in Zirconium Alloy Oxide Film |
| WANG Xiaoqi, ZHANG Jinhu, GUO Hui, LI Xuexiong, XU Haisheng, BAI Chunguang, XU Dongsheng, YANG Rui |
| 图8 氧化膜中平行于氧化物-金属界面的裂纹演化模拟得到的拉伸力-位移曲线 |
| Fig.8 Force-displacement curve for crack parallel to the oxide-metal interface by simulation |
|