锆合金氧化膜中相变与裂纹演化的相场模拟
王小齐, 张金虎, 郭辉, 李学雄, 许海生, 柏春光, 徐东生, 杨锐

Phase-Field Simulations of Phase Transformation and Crack Evolution in Zirconium Alloy Oxide Film
WANG Xiaoqi, ZHANG Jinhu, GUO Hui, LI Xuexiong, XU Haisheng, BAI Chunguang, XU Dongsheng, YANG Rui
图2 m-ZrO2晶粒长大过程中的形貌演化
Fig.2 Grain growth process and evolution of the morphology of m-ZrO2 (η—non-conserved order parameter, t—time)
(a) t = 1.0 × 10-12 s (b) t = 6.0 × 10-8 s (c) t = 1.0 × 10-7 s (d) t = 3.0 × 10-7 s