搅拌摩擦加工改性Mg-5Zn合金的显微组织与耐腐蚀性能 |
| 龙飞, 刘瞿, 朱艺星, 周梦然, 陈高强, 史清宇 |
|
Microstructure and Corrosion Resistance of Modified Mg-5Zn Alloy via Friction Stir Processing |
| LONG Fei, LIU Qu, ZHU Yixing, ZHOU Mengran, CHEN Gaoqiang, SHI Qingyu |
| 图4 铸态Mg-5Zn合金和FSP处理样品的XRD谱 |
| Fig.4 XRD spectra of as-cast and FSP-treated Mg-5Zn alloy samples |
|