搅拌摩擦加工改性Mg-5Zn合金的显微组织与耐腐蚀性能 |
| 龙飞, 刘瞿, 朱艺星, 周梦然, 陈高强, 史清宇 |
|
Microstructure and Corrosion Resistance of Modified Mg-5Zn Alloy via Friction Stir Processing |
| LONG Fei, LIU Qu, ZHU Yixing, ZHOU Mengran, CHEN Gaoqiang, SHI Qingyu |
| 图2 3种轴肩直径下搅拌摩擦加工(FSP)处理的Mg-5Zn合金样品的反极图 |
| Fig.2 Inverse pole figures of Mg-5Zn alloys treated by friction stir processing (FSP) with shoulder diameters of 14 mm (a), 17 mm (b), and 20 mm (c) named FSP-14, FSP-17, and FSP-20, respectively (ND—normal direction, TD—transverse direction) |
|