一种新型Ti-Al-Mn-Nb合金的固态相变行为
王强, 李小兵, 郝俊杰, 陈波, 张滨, 张二林, 刘奎

Solid-State Phase Transformation Behavior of a Novel Ti-Al-Mn-Nb Alloy
WANG Qiang, LI Xiaobing, HAO Junjie, CHEN Bo, ZHANG Bin, ZHANG Erlin, LIU Kui
表1 图3中各相的EPMA点分析结果 (atomic fraction / %)
Table 1 Point analysis results of phases in Fig.3
PhaseTiAlMnNbSi
βo56.9533.444.913.980.72
α2/γ50.9244.801.432.650.20
γ49.4745.281.823.110.32