一种新型Ti-Al-Mn-Nb合金的固态相变行为 |
| 王强, 李小兵, 郝俊杰, 陈波, 张滨, 张二林, 刘奎 |
|
Solid-State Phase Transformation Behavior of a Novel Ti-Al-Mn-Nb Alloy |
| WANG Qiang, LI Xiaobing, HAO Junjie, CHEN Bo, ZHANG Bin, ZHANG Erlin, LIU Kui |
| 图8 在不同温度保温30 min并水淬后Ti-Al-Mn-Nb合金中β、α、γ相体积分数统计结果 |
| Fig.8 Phase volume fraction results of β, α, and γ phases in water quenched Ti-Al-Mn-Nb alloy after holding at different temperatures for 30 min |
|