一种新型Ti-Al-Mn-Nb合金的固态相变行为 |
| 王强, 李小兵, 郝俊杰, 陈波, 张滨, 张二林, 刘奎 |
|
Solid-State Phase Transformation Behavior of a Novel Ti-Al-Mn-Nb Alloy |
| WANG Qiang, LI Xiaobing, HAO Junjie, CHEN Bo, ZHANG Bin, ZHANG Erlin, LIU Kui |
| 图7 在不同温度下保温30 min并水淬后Ti-Al-Mn-Nb合金的EBSD相分布图和极图 |
| Fig.7 EBSD phase maps (a-c) and pole figures (d-f) of water quenched Ti-Al-Mn-Nb alloy after holding at 1240 oC (a, d), 1200 oC (b, e), and 1160 oC (c, f) for 30 min, respectively |
|