一种低成本第三代单晶高温合金的高温氧化行为 |
| 李永梅, 谭子昊, 王新广, 陶稀鹏, 杨彦红, 刘纪德, 刘金来, 李金国, 周亦胄, 孙晓峰 |
|
Oxidation Behavior of a Low-Cost Third-Generation Ni-Based Single-Crystal Superalloy |
| LI Yongmei, TAN Zihao, WANG Xinguang, TAO Xipeng, YANG Yanhong, LIU Jide, LIU Jinlai, LI Jinguo, ZHOU Yizhou, SUN Xiaofeng |
| 图9 合金1150 ℃连续氧化增重曲线与合金经1120 ℃非连续氧化100 h后的剥落氧化皮形貌 |
| Fig.9 Mass gain curve of the experimental alloy after continuous oxidizing at 1150 oC (a) and photo of peeling oxide of alloy after discontinous oxidizing at 1120 oC for 100 h (b) |
|