一种低成本第三代单晶高温合金的高温氧化行为 |
| 李永梅, 谭子昊, 王新广, 陶稀鹏, 杨彦红, 刘纪德, 刘金来, 李金国, 周亦胄, 孙晓峰 |
|
Oxidation Behavior of a Low-Cost Third-Generation Ni-Based Single-Crystal Superalloy |
| LI Yongmei, TAN Zihao, WANG Xinguang, TAO Xipeng, YANG Yanhong, LIU Jide, LIU Jinlai, LI Jinguo, ZHOU Yizhou, SUN Xiaofeng |
| 图5 合金经1120 ℃氧化不同时间后样品纵截面的氧化层结构演化 |
| Fig.5 SEM images of longitudinal section of samples after oxidizing at 1120 oC for 1 h (a), 5 h (b), 40 h (c), 100 h (d), and 200 h (e) (ORD—oxdation reaction domain) |
|