一种低成本第三代单晶高温合金的高温氧化行为 |
| 李永梅, 谭子昊, 王新广, 陶稀鹏, 杨彦红, 刘纪德, 刘金来, 李金国, 周亦胄, 孙晓峰 |
|
Oxidation Behavior of a Low-Cost Third-Generation Ni-Based Single-Crystal Superalloy |
| LI Yongmei, TAN Zihao, WANG Xinguang, TAO Xipeng, YANG Yanhong, LIU Jide, LIU Jinlai, LI Jinguo, ZHOU Yizhou, SUN Xiaofeng |
| 图2 合金在1120 ℃下氧化10和200 h的氧化增重曲线 |
| Fig.2 Curves of mass gain vs oxidation time (t) in the early 10 h (a) and in 200 h (b) |
|