一种低成本第三代单晶高温合金的高温氧化行为 |
| 李永梅, 谭子昊, 王新广, 陶稀鹏, 杨彦红, 刘纪德, 刘金来, 李金国, 周亦胄, 孙晓峰 |
|
Oxidation Behavior of a Low-Cost Third-Generation Ni-Based Single-Crystal Superalloy |
| LI Yongmei, TAN Zihao, WANG Xinguang, TAO Xipeng, YANG Yanhong, LIU Jide, LIU Jinlai, LI Jinguo, ZHOU Yizhou, SUN Xiaofeng |
| 图1 标准热处理工艺流程图 |
| Fig.1 Schematic of the standard heat treatment regime (AC—air cooling) |
|