Nb含量和均质化处理对奥氏体不锈钢铸态组织和力学性能的影响
谢昂, 陈胜虎, 姜海昌, 戎利建

Effects of Nb Content and Homogenization Treatment on the Microstructure and Mechanical Properties of Cast Austenitic Stainless Steel
XIE Ang, CHEN Shenghu, JIANG Haichang, RONG Lijian
图4 不同Nb含量奥氏体不锈钢室温拉伸断口形貌的SEM像
Fig.4 Low (a, c, e) and high (b, d, f) magnified SEM images of fracture surfaces of 0Nb (a, b), 3Nb (c, d), and 9Nb (e, f) steel samples after tensile test at room temperature (Inset in Fig.4f shows the EDS area scan mapping of rectangular zone)