Nb含量和均质化处理对奥氏体不锈钢铸态组织和力学性能的影响 |
| 谢昂, 陈胜虎, 姜海昌, 戎利建 |
|
Effects of Nb Content and Homogenization Treatment on the Microstructure and Mechanical Properties of Cast Austenitic Stainless Steel |
| XIE Ang, CHEN Shenghu, JIANG Haichang, RONG Lijian |
| 图1 不同Nb含量奥氏体不锈钢铸态组织的OM像和SEM像 |
| Fig.1 OM (a-c) and SEM (d-f) images of 0Nb (a, d), 3Nb (b, e), and 9Nb (c, f) steel samples |
|