Mn偏析对0.3C-11Mn-2.7Al-1.8Si-Fe中锰钢力学性能的影响及作用机制
蔡星周, 刘胜杰, 张禹森, 李小龙, 张宇鹤, 张文彬, 陈雷, 金淼

Effect of Mn Segregation on Mechanical Properties of 0.3C-11Mn-2.7Al-1.8Si-Fe Medium Mn Steel and Its Mechanism
CAI Xingzhou, LIU Shengjie, ZHANG Yusen, LI Xiaolong, ZHANG Yuhe, ZHANG Wenbin, CHEN Lei, JIN Miao
图9 S1和S2样品断口形貌的SEM像
Fig.9 Low (a, c) and high (b, d) magnified SEM images of S1 (a, b) and S2 (c, d) samples