Mn偏析对0.3C-11Mn-2.7Al-1.8Si-Fe中锰钢力学性能的影响及作用机制 |
| 蔡星周, 刘胜杰, 张禹森, 李小龙, 张宇鹤, 张文彬, 陈雷, 金淼 |
|
Effect of Mn Segregation on Mechanical Properties of 0.3C-11Mn-2.7Al-1.8Si-Fe Medium Mn Steel and Its Mechanism |
| CAI Xingzhou, LIU Shengjie, ZHANG Yusen, LI Xiaolong, ZHANG Yuhe, ZHANG Wenbin, CHEN Lei, JIN Miao |
| 图4 S1样品微观组织的SEM像和Mn元素的EDS线扫描结果 |
| Fig.4 SEM images of S1 sample (a) and corresponding EDS line scanning result of Mn (b) |
|