fccbcc钢板在超高速撞击下的微观组织差异
孙欢腾, 马运柱, 蔡青山, 王健宁, 段有腾, 张梦祥

Differential Microstructure Between fcc and bcc Steel Plates Under Hyper-Velocity Impact
SUN Huanteng, MA Yunzhu, CAI Qingshan, WANG Jianning, DUAN Youteng, ZHANG Mengxiang
图11 Q345钢板穿孔径向处(图1b2中位置5)的EBSD表征结果
Fig.11 EBSD characterizations for the sample near perforation of Q345 steel at positon 5 in Fig.1b2
(a) inverse pole figure (IPF) along ND
(b) phase distribution map
(c) <110> silk texture parallel to ND
(d) kernel average misorientation (KAM) map
(e) dynamic recrystallization distribution map
(f) relative frequency distribution of local misorientation angle within a certain angle range of 0°-5°