fcc和bcc钢板在超高速撞击下的微观组织差异 |
| 孙欢腾, 马运柱, 蔡青山, 王健宁, 段有腾, 张梦祥 |
|
Differential Microstructure Between fcc and bcc Steel Plates Under Hyper-Velocity Impact |
| SUN Huanteng, MA Yunzhu, CAI Qingshan, WANG Jianning, DUAN Youteng, ZHANG Mengxiang |
| 图7 304不锈钢穿孔附近不同位置(图1a2中位置1~4)织构所占的面积分数 |
| Fig.7 Texture area fractions for the sample near perforation of 304 stainless steel at positons 1-4 in Fig.1a2 (S—{123}< |
|