表1 计算采用的Mg-6%Al合金热物性参数[13]
Table 1 Thermophysical properties of Mg-6%Al alloy used in the calculations[13]
ParameterValueUnit
Diffusivity of alloy elements in liquid DL1.8 × 10-9m2·s-1
Diffusivity of alloy elements in solid DS1.0 × 10-13m2·s-1
Liquidus temperature TL901K
Partition coefficient k0.4-
Liquidus slope mL-5.5K·%-1 (% for mass fraction)
Gibbs-Thomson coefficient Γ2.0 × 10-7K·m
Kinetic anisotropy δk0.5-
Thermodynamic anisotropy δ0.03-
Accommodation coefficient γ1.25-
Degree of anisotropy n6-