六重对称合金枝晶生长场变量扩散元胞自动机模型 |
| 汤思璠, 魏晶晶, 岳怡心, 李鹏宇, 姚曼, 王旭东 |
|
Field-Variable Diffusion Cellular Automaton Model for Dendritic Growth with Sixfold Symmetry Alloys |
| TANG Sifan, WEI Jingjing, YUE Yixin, LI Pengyu, YAO Man, WANG Xudong |
| 图1 Von Neumann型邻胞2种模型模拟结果 |
| Fig.1 Morphologies simulated by two cellular automaton (CA) models using Von Neumann neighborhood (a1-a3) original CA model with 20 iterations (a1), 60 iterations (a2), and 100 iterations (a3) (b1-b3) field variable diffusion (FCA) model with 120 iterations (b1), 260 iterations (b2), and 400 iterations (b3) |
|