含Cr耐蚀钢筋在模拟高碱性混凝土孔隙液中的钝化行为 |
| 王慕亮, 孙玉朋, 陈磊, 魏洁, 董俊华 |
|
Passive Behavior of Corrosion-Resistant Cr-Containing Steel Bars in Simulated High-Alkaline Concrete Pore Solution |
| WANG Muliang, SUN Yupeng, CHEN Lei, WEI Jie, DONG Junhua |
| 图7 20MnSi、3Cr和9Cr钢极化电阻(Rc)和电荷转移电阻(Ra)随时间变化曲线 |
| Fig.7 Evolutions of Rc (a) and Ra (b) of 20MnSi, 3Cr, and 9Cr steels with time |
|