含Cr耐蚀钢筋在模拟高碱性混凝土孔隙液中的钝化行为 |
| 王慕亮, 孙玉朋, 陈磊, 魏洁, 董俊华 |
|
Passive Behavior of Corrosion-Resistant Cr-Containing Steel Bars in Simulated High-Alkaline Concrete Pore Solution |
| WANG Muliang, SUN Yupeng, CHEN Lei, WEI Jie, DONG Junhua |
| 图2 20MnSi、3Cr和9Cr钢在模拟混凝土孔隙液中开路电位随浸泡时间的变化 |
| Fig.2 Open circuit potential (Eocp) of 20MnSi, 3Cr, and 9Cr steels with immersion time in simulated concrete pore solution (SCE—saturated calomel electrode) |
|