阴极保护条件对高压直流干扰下X80钢腐蚀行为的影响规律及作用机制 |
| 谷少杰, 刘洋, 李彩霞, 胡上茂, 杜艳霞 |
|
Effect and Mechanism of Cathodic Protection Conditions on the Corrosion Behavior of X80 Steel Under HVDC Interference |
| GU Shaojie, LIU Yang, LI Caixia, HU Shangmao, DU Yanxia |
| 图10 不同阴极保护极化电位阴极保护4 d后试样表面微观形貌及EDS分析结果 |
| Fig.10 Surface micromorphologies (a1, a2, b1, c1, d1, d2) and corresponding EDS analyses (a3, b2, c2, d3) of samples after cathodic protection at different cathodic protection polarization poten-tials for 4 d (a1, a2, a3) -0.85 V (b1, b2) -0.95 V (c1, c2) -1.05 V (d1, d2, d3) -1.20 V |
|