阴极保护条件对高压直流干扰下X80钢腐蚀行为的影响规律及作用机制 |
| 谷少杰, 刘洋, 李彩霞, 胡上茂, 杜艳霞 |
|
Effect and Mechanism of Cathodic Protection Conditions on the Corrosion Behavior of X80 Steel Under HVDC Interference |
| GU Shaojie, LIU Yang, LI Caixia, HU Shangmao, DU Yanxia |
| 图4 不同阴保电位直流干扰后及酸洗后试样的宏观腐蚀形貌 |