阴极保护条件对高压直流干扰下X80钢腐蚀行为的影响规律及作用机制 |
| 谷少杰, 刘洋, 李彩霞, 胡上茂, 杜艳霞 |
|
Effect and Mechanism of Cathodic Protection Conditions on the Corrosion Behavior of X80 Steel Under HVDC Interference |
| GU Shaojie, LIU Yang, LI Caixia, HU Shangmao, DU Yanxia |
| 图3 不同阴极保护极化电位条件下阴极保护4 d后试样的表面宏观形貌 |
| Fig.3 Macroscopic morphologies of the specimen surface after cathodic protection with different cathodic protection potentials for 4 d (a) -0.85 V (b) -0.95 V (c) -1.05 V (d) -1.20 V |
|