| 李夫顺, 刘志鹏, 丁灿灿, 胡斌, 罗海文 |
|
Strengthening and Plastifying Mechanisms of a Novel High-Strength Low-Density Austenitic Steel |
| LI Fushun, LIU Zhipeng, DING Cancan, HU Bin, LUO Haiwen |
| 图5 35CR-T和75CR-AT样品中3种强化机制对屈服强度增量贡献的对比 |
| Fig.5 Comparison on the contribution of three strengthening mechanisms to increment of yield strength in 35CR-T and 75CR-AT specimens (Δσg—grain refinement strengthening increment, Δσd—dislocation hardening increment, Δσp—precipitation hardening increment) |
|