Zr61Ti2Cu25Al12 非晶合金的过冷液体特性与晶化解耦 |
| 李晓诚, 寇生中, 李春玲, 李春燕, 赵燕春 |
|
Supercooled Liquid Characteristics and Crystallization Decoupling of Zr61Ti2Cu25Al12 Amorphous Alloy |
| LI Xiaocheng, KOU Shengzhong, LI Chunling, LI Chunyan, ZHAO Yanchun |
| 图7 解耦指数(ξ)与脆度系数(m)之间的关系 |
| Fig.7 Decoupling exponent (ξ) representing the decoupling of crystal growth kinetics from viscous flow plotted as a function of the supercooled liquid m (GST—Ge2Sb2Te5) |
|