Zr61Ti2Cu25Al12 非晶合金的过冷液体特性与晶化解耦 |
| 李晓诚, 寇生中, 李春玲, 李春燕, 赵燕春 |
|
Supercooled Liquid Characteristics and Crystallization Decoupling of Zr61Ti2Cu25Al12 Amorphous Alloy |
| LI Xiaocheng, KOU Shengzhong, LI Chunling, LI Chunyan, ZHAO Yanchun |
| 图6 本工作及相关文献[ |
| Fig.6 Angell plot for reduced temperature dependence of viscosity in several representative glass forming liquids[ |
|