Zr61Ti2Cu25Al12 非晶合金的过冷液体特性与晶化解耦 |
| 李晓诚, 寇生中, 李春玲, 李春燕, 赵燕春 |
|
Supercooled Liquid Characteristics and Crystallization Decoupling of Zr61Ti2Cu25Al12 Amorphous Alloy |
| LI Xiaocheng, KOU Shengzhong, LI Chunling, LI Chunyan, ZHAO Yanchun |
| 图5 Zr61Ti2Cu25Al12合金特征温度的Kissinger图及经时间维度调整后的曲线 |
| Fig.5 Kissinger plots for characteristic temperatures of Zr61Ti2Cu25Al12 metallic glass (a) and adjusted with proper time dimension shift (b) (U─crystal growth rate; η─viscosity; Ukin─kinetic coefficient for crystal growth; Tc─characteristic temperatures Tg, Tx, and Tp) |
|