Zr61Ti2Cu25Al12 非晶合金的过冷液体特性与晶化解耦 |
| 李晓诚, 寇生中, 李春玲, 李春燕, 赵燕春 |
|
Supercooled Liquid Characteristics and Crystallization Decoupling of Zr61Ti2Cu25Al12 Amorphous Alloy |
| LI Xiaocheng, KOU Shengzhong, LI Chunling, LI Chunyan, ZHAO Yanchun |
| 图1 直径为3 mm Zr61Ti2Cu25Al12合金铸态棒的XRD谱和HRTEM像 |
| Fig.1 XRD spectrum (a) and HRTEM image (Inset shows selected area electron diffraction (SAED) pattern) (b) of Zr61Ti2Cu25Al12 as-cast rod with a diameter of 3 mm |
|