稀土Y掺杂V-Cr合金增塑机理及透氢性能 |
| 杨波, 陈小亮, 史晓斌, 任伟, 高恒, 宋广生 |
|
Softening Mechanism and Hydrogen Permeability of Rare Earth Y-Doped V-Cr Alloys |
| YANG Bo, CHEN Xiaoliang, SHI Xiaobin, REN Wei, GAO Heng, SONG Guangsheng |
| 图10 铸态V-Cr和V-Cr-Y合金的硬度和最大冷轧压下率 |
| Fig.10 Vickers hardnesses and nanoindentation hardnesses of matrix (a) and maximum cold-rolling reduction rate (b) of as-cast V-Cr and V-Cr-Y alloys |
|