稀土Y掺杂V-Cr合金增塑机理及透氢性能 |
| 杨波, 陈小亮, 史晓斌, 任伟, 高恒, 宋广生 |
|
Softening Mechanism and Hydrogen Permeability of Rare Earth Y-Doped V-Cr Alloys |
| YANG Bo, CHEN Xiaoliang, SHI Xiaobin, REN Wei, GAO Heng, SONG Guangsheng |
| 图3 不同Cr、Y含量铸态钒合金的XRD谱 |
| Fig.3 XRD spectra of as-cast V alloys (Dash lines show the pure vanadium diffraction peaks) |
|